二铝酸钙加入量对刚玉浇注料性能的影响
秦红彬, 金锋, 唐世明, 周慧君, 李红霞, 石书冰, 张三华, 程立, 惠先磊
Effect of calcium dialuminate addition on properties of corundum castables
Qin Hongbin, Jin Feng, Tang Shiming, Zhou Huijun, Li Hongxia, Shi Shubing, Zhang Sanhua, Cheng Li, Hui Xianlei
耐火材料 . 2023, (3): 189 -193 .  DOI: 10.3969/j.issn.1001-1935.2023.03.002