煤矸石陶粒替代开孔珍珠岩骨料制备轻质铝硅系浇注料
昝文宇, 马北越, 王玉清, 蒋志峰
Preparation of lightweight alumina-silica castables by replacing open-pore perlite aggregates with coal gangue ceramsite
Zan Wenyu, Ma Beiyue, Wang Yuqing, Jiang Zhifeng
耐火材料 . 2023, (3): 205 -209 .  DOI: 10.3969/j.issn.1001-1935.2023.03.005