结合剂种类对刚玉-尖晶石浇注料抗镍基高温合金侵蚀性能的影响
潘元帅, 王刚, 冯海霞, 柳军, 田朋丹, 韩艺辉, 王建斌
Effect of binder type on corrosion resistance to nickel-based superalloy of corundum-spinel castables
Pan Yuanshuai, Wang Gang, Feng Haixia, Liu Jun, Tian Pengdan, Han Yihui, Wang Jianbin
耐火材料
.
2023, (3): 220
-225
.
DOI: 10.3969/j.issn.1001-1935.2023.03.008