凝胶注模-固相反应法制备硼酸铝多孔陶瓷
李鑫, 李昊明, 张强, 曹岳岐, 刘幸儿, 郭安然
Preparation of porous aluminum borate ceramics by gel casting-solid state reaction method
Li Xin, Li Hao-ming, Zhang Qiang, Cao Yueqi, Liu Xing’er, Guo Anran
耐火材料 . 2023, (4): 277 -280 .  DOI: 10.3969/j.issn.1001-1935.2023.04.001