热处理温度对矾土基莫来石材料结构及晶体生长的影响
麦海香, 赵飞, 安建成, 王亚利, 连伟康胡杨, 葛铁柱, 刘新红
Effect of heat-treatment temperature on crystal growth and structure of bauxite based mullite materials
Mai Haixiang, Zhao Fei, An Jiancheng, Wang Yali, Lian Weikang, Hu Yang, Ge Tiezhu, Liu Xinhong
耐火材料
.
2023, (4): 314
-319
.
DOI: 10.3969/j.issn.1001-1935.2023.04.009