钛铁渣加入量对Al 2O 3-SiC-C铁沟浇注料性能的影响
龙图, 顾华志, 张美杰, 黄奥, 邱文冬
Effects of ferrotitanium slag addition on properties of Al 2O 3-SiC-C iron trough castables
Long Tu, Gu Huazhi, Zhang Meijie, Huang Ao, Qiu Wendong
耐火材料 . 2023, (4): 351 -355 .  DOI: 10.3969/j.issn.1001-1935.2023.04.016