钒钛磁铁矿熔渣与耐火材料间的相互作用
高伟, 刘朝阳, 马北越, 韦善, 于景坤
Interaction between vanadium titanomagnetite slag and refractories
Gao Wei, Liu Zhaoyang, Ma Beiyue, Wei Shan, Yu Jingkun
耐火材料 . 2023, (4): 365 -368 .  DOI: 10.3969/j.issn.1001-1935.2023.04.019