先进耐火材料创新助推国家战略实施
李红霞
Advanced refractories innovation boosts China’s strategy implementation
Li Hongxia
耐火材料 . 2023, (5): 369 -376 .  DOI: 10.3969/j.issn.1001-1935.2023.05.001