钢铁工业用耐火材料新技术进展
王战民, 曹喜营, 吴吉光, 秦红彬, 李志刚, 余同暑, 柳军, 刘国齐, 段斌文, 王自强
New technology progress of refractories for iron and steel industry
Wang Zhanmin, Cao Xiying, Wu Jiguang, Qin Hongbin, Li Zhigang, Yu Tongshu, Liu Jun, Liu Guoqi, Duan Binwen, Wang Ziqiang
耐火材料 . 2023, (5): 377 -385 .  DOI: 10.3969/j.issn.1001-1935.2023.05.002