陶瓷介质滤波器表面斑点分析及解决措施
周会俊, 罗天, 王龙光, 牛世程, 王建坤, 禄向阳
Analysis and countermeasures of surface spots on ceramic dielectric filters
Zhou Huijun, Luo Tian, Wang Longguang, Niu Shicheng, Wang Jiankun, Lu Xiangyang
耐火材料 . 2023, (5): 431 -433 .  DOI: 10.3969/j.issn.1001-1935.2023.05.012