光固化3D打印制备莫来石纤维基多孔陶瓷
李鑫, 曹岳岐, 张强, 郭安然
Preparation of mullite fiber based porous ceramics via photocuring 3D printing
Li Xin, Cao Yueqi, Zhang Qiang, Guo Anran
耐火材料 . 2023, (6): 461 -466 .  DOI: 10.3969/j.issn.1001-1935.2023.06.001