CA 6质耐火材料在水泥回转窑过渡带的应用及损毁机制
李斌, 刘杰, 朱波, 郭玉涛, 任博, 封吉圣, 陈俊红
Application and damage mechanism of CA 6 refractories in transition zone of cement rotary kilns
Li Bin, Liu Jie, Zhu Bo, Guo Yutao, Ren Bo, Feng Jisheng, Chen Junhong
耐火材料 . 2023, (6): 479 -483 .  DOI: 10.3969/j.issn.1001-1935.2023.06.004