锂离子电池正极材料用莫来石溶胶结合匣钵材料的性能研究
鞠茂奇, 程水明, 夏昌勇, 梁永和, 丛培源, 聂建华
Properties of sagger materials bonded by mullite-sol for cathode materials of lithium ion batteries
Ju Maoqi, Cheng Shuiming, Xia Changyong, Liang Yonghe, Cong Peiyuan, Nie Jianhua
耐火材料
.
2023, (6): 495
-499
.
DOI: 10.3969/j.issn.1001-1935.2023.06.007