锆英石加入量对低碳镁碳砖抗剥落性能的影响
郑俊国, 赵伟, 黄奥, 顾华志, 孙春晖颜浩, 刘靖轩, 赵现堂
Effect of zircon addition on spalling resistance of low-carbon MgO-C bricks
Zheng Junguo, Zhao Wei, Huang Ao, Gu Huazhi, Sun Chunhui, Liu Jingxuan, Yan Hao, Zhao Xiantang
耐火材料
.
2023, (6): 508
-513
.
DOI: 10.3969/j.issn.1001-1935.2023.06.010