废旧高铝砖在LF精炼渣中的溶解行为研究
慕鑫, 贾毅, 刘春阳, 柴光伟, 余吴明, 杜传明, 马北越
Dissolution behavior of waste high-alumina bricks in LF refining slag
Mu Xin, Jia Yi, Liu Chunyang, Chai Guangwei, Yu Wuming, Du Chuanming, Ma Beiyue
耐火材料 . 2024, (1): 25 -29 .  DOI: 10.3969/j.issn.1001-1935.2024.01.005