铜冶炼侧吹炉用镁铬质耐火材料损毁机制
付琪琪, 钟立桦, 白文献, 淦永彤, 邓俊杰
Damage mechanism of magnesia-chrome refractories for side-blown copper smelting furnace
Fu Qiqi, Zhong Lihua, Bai Wenxian, Gan Yongtong, Deng Junjie
耐火材料 . 2024, (2): 148 -154 .  DOI: 10.3969/j.issn.1001-1935.2024.02.011