SiO 2-Al 2O 3复合气凝胶常压干燥制备技术研究进展
王指正, 郭玉香, 杨晓东, 孙培凇
Research progress of ambient pressure drying preparation technology of SiO 2-Al 2O 3 composite aerogel
Wang Zhizheng, Guo Yuxiang, Yang Xiaodong, Sun Peisong
耐火材料 . 2024, (2): 179 -184 .  DOI: 10.3969/j.issn.1001-1935.2024.02.016