CaO对MgAl
2O
4材料和ZrO
2-MgAl
2O
4材料侵蚀机制研究
刘中飞, 吴锋, 李心慰, 梁效诚, 罗旭东, 钱国华
Corrosion mechanisms of CaO to MgAl
2O
4 materials and ZrO
2-MgAl
2O
4 materials
Liu Zhongfei, Wu Feng, Li Xinwei, Liang Xiaocheng, Luo Xudong, Qian Guohua
耐火材料
.
2024, (3): 199
-203
.
DOI: 10.3969/j.issn.1001-1935.2024.03.004