Preparation of calcium zirconate materials by two-step sintering
Wang Meng, Wen Shuhua, Yu Jingkun, Yuan Lei, Wen Tianpeng
耐火材料 . 2024, (3): 204 -207 .  DOI: 10.3969/j.issn.1001-1935.2024.03.005