菱镁矿除杂提质研究进展
齐笑, 付亮亮, 白丁荣, 许光文
Research progress on impurity removal and quality improvement of magnesite
Qi Xiao, Fu Liangliang, Bai Dingrong, Xu Guangwen
耐火材料 . 2024, (3): 257 -262 .  DOI: 10.3969/j.issn.1001-1935.2024.03.016