氧化铝气凝胶的耐温性能研究
任河, 佟天白, 刘梅, 王利娜, 范召东
Temperature resistance of alumina aerogels
Ren He, Tong Tianbai, Liu Mei, Wang Lina, Fan Zhaodong
耐火材料 . 2024, (4): 297 -301 .  DOI: 10.3969/j.issn.1001-1935.2024.04.004