酚醛/环氧树脂凝胶注模成型制备反应烧结碳化硅
凌厦厦, 相宇博, 郑翰, 吴吉光
Fabrication of reaction-bonded silicon carbide via phenolic/epoxy resin gelcasting
Ling Xiaxia, Xiang Yubo, Zheng Han, Wu Jiguang
耐火材料 . 2024, (4): 329 -333 .  DOI: 10.3969/j.issn.1001-1935.2024.04.010