莫来石-刚玉-镁铝尖晶石复相材料的抗碱侵蚀性能研究
高云琴, 郭凯歌, 马爱琼, 牛兴荣, 杨光, 张旭东
Preparation and alkali corrosion resistance of mullite-corundum-magnesium aluminate spinel multiphase materials
Gao Yunqin, Guo Kaige, Ma Aiqiong, Niu Xingrong, Yang Guang, Zhang Xudong
耐火材料 . 2024, (4): 334 -340 .  DOI: 10.3969/j.issn.1001-1935.2024.04.011