以蔗糖为碳源制备亚微米级TiB
2粉体的研究
王兴国, 陈滨, 李欣, 长世伦, 徐晨, 杨建红
Preparation of submicron TiB
2 powder using sucrose as carbon source
Wang Xingguo, Chen Bin, Li Xin, Chang Shilun, Xu Chen, Yang Jianhong
耐火材料
.
2024, (5): 405
-409
.
DOI: 10.3969/j.issn.1001-1935.2024.05.007