稀土氧化物对低温固相合成镁铝尖晶石纤维的影响
郭江鹏, 邓长宇, 王昕悦, 陈昕煜, 段红娟, 张海军
Effects of rare earth oxides on low temperature solid phase synthesis of MgAl
2O
4 fibers
Guo Jiangpeng, Deng Changyu, Wang Xinyue, Chen Xinyu, Duan Hongjuan, Zhang Haijun
耐火材料
.
2024, (5): 410
-413
.
DOI: 10.3969/j.issn.1001-1935.2024.05.008