AOD脱铁提镍工艺用镁碳砖的侵蚀机制
李振, 齐江涛, 谭建兴, 郑俊国, 李院高
Corrosion mechanism of MgO-C bricks for AOD deferrization and nickel extraction process
Li Zhen, Qi Jiangtao, Tan Jianxing, Zheng Junguo, Li Yuangao
耐火材料 . 2024, (5): 431 -435 .  DOI: 10.3969/j.issn.1001-1935.2024.05.012