欧冶炉竖炉围管用Si 3N 4结合SiC砖的损毁分析
赵馨雨, 杨文刚, 穆元冬, 田果, 吴吉光, 相宇博, 叶国田
Damage analysis of Si 3N 4 bonded SiC bricks for bustle pipes of OY shaft furnaces
耐火材料 . 2024, (6): 513 -516 .  DOI: 10.3969/j.issn.1001-1935.2024.06.010