基于卷积神经网络的电熔镁砂块料识别与分类
赵鑫, 岳静静, 游杰刚, 张小芳, 冯东, 侯庆冬, 张玲, 邓承继
Identification and classification of fused magnesia blocks based on convolutional neural network
耐火材料 . 2024, (6): 517 -520 .  DOI: 10.3969/j.issn.1001-1935.2024.06.011