基于生命周期评价方法的硅莫砖碳足迹分析与减碳路径研究
马晓, 尹超男, 王俊涛, 张晋, 胡建辉
Carbon footprint analysis and carbon reduction path research of silicon carbide-mullite bricks based on life cycle assessment
耐火材料 . 2024, (6): 521 -526 .  DOI: 10.3969/j.issn.1001-1935.2024.06.012