h-BN对低碳Al 2O 3-C耐火材料性能的影响
罗益欣, 王杏, 刘正龙, 余超, 邓承继, 丁军
Effect of h-BN on properties of low carbon Al 2O 3-C refractories
Luo Yixin, Wang Xing, Liu Zhenglong, Yu Chao, Deng Chengji, Ding Jun
耐火材料 . 2025, (1): 13 -18 .  DOI: 10.3969/j.issn.1001-1935.2025.01.003