65~69工艺参数对Al 2O 3-C耐火材料抗氧化性和抗水化性的影响
张瑞, 孙旭东, 魏瀚, 袁彪, 王俊涛袁林, 刘士范, 陈松林
Effect of process parameters on oxidation resistance and hydration resistance of Al 2O 3-C refractories
Zhang Rui, Sun Xudong, Wei Han, Yuan Biao, Wang Juntao, Yuan Lin, Liu Shifan, Chen Songlin
耐火材料 . 2025, (1): 65 -69 .  DOI: 10.3969/j.issn.1001-1935.2025.01.012