镁碳质耐火材料的损毁机制及性能研究进展
王圣博, 侯庆冬, 田吉, 罗旭东, 马北越, 李季佳, 满斯林
Research progress on damage mechanism and performance of magnesia-carbon refractories
Wang Shengbo, Hou Qingdong, Tian Ji, Luo Xudong, Ma Beiyue, Li Jijia, Man Silin
耐火材料 . 2025, (3): 259 -265 .  DOI: 10.3969/j.issn.1001-1935.2025.03.015