短切玻璃纤维对硅溶胶结合刚玉质浇注料性能的影响
丁宇航, 刘会永, 魏建修, 熊继全, 项冰, 夏昌勇
Effects of chopped glass fibers on properties of silica sol bonded corundum castables
Ding Yuhang, Liu Hui-yong, Wei Jianxiu, Xiong Jiquan, Xiang Bing, Xia Changyong
耐火材料 . 2025, (4): 283 -288 .  DOI: 10.3969/j.issn.1001-1935.2025.04.002