含纳米CaCO
3的刚玉-尖晶石浇注料显微结构及抗热震性能的研究
谭丹, 王景然, 张锦化, 倪月娥, 韩兵强
Microstructure and thermal shock resistance of corundum-spinel castables containing nano-CaCO
3
Tan Dan, Wang Jingran, Zhang Jinhua, Ni Yue’e, Han Bingqiang
耐火材料
.
2025, (4): 330
-336
.