氮基耐火材料与氧化镧和铝酸镧的界面反应研究
马飞祥, 李红霞, 刘国齐, 顾强
Interfacial reactions of nitrogen-based refractories with lanthanum oxide and lanthanum aluminate
Ma Fei-xiang, Li Hongxia, Liu Guoqi, Gu Qiang
耐火材料
.
2025, (5): 369
-374
.
DOI: 10.3969/j.issn.1001-1935.2025.05.001