石墨材料抗氧化MoSi 2-CrB 2-SiC-Si复合涂层的制备及性能研究
杨佳妮, 郭晓阳, 姜岩
Preparation and performance of anti-oxidation MoSi 2-CrB 2-SiC-Si composite coating for graphite materials
Yang Jiani, Guo Xiaoyang, Jiang Yan
耐火材料 . 2025, (5): 398 -405 .  DOI: 10.3969/j.issn.1001-1935.2025.05.006