煤气化炉渣碳热还原氮化合成SiAlON复合粉体的研究
郭世萌, 尹洪峰, 贾换, 辛亚楼, 汤云, 袁蝴蝶, 任小虎
Synthesis of SiAlON composite powders by carbothermal reduction and nitridation of coal gasification slag
Guo Shimeng, Yin Hongfeng, Jia Huan, Xin Yalou, Tang Yun, Yuan Hudie, Ren Xiaohu
耐火材料 . 2025, (6): 466 -470 .  DOI: 10.3969/j.issn.1001-1935.2025.06.002