铝碳复合滑板再生料加入量对Al
2O
3-SiC-C浇注料性能的影响
陈聪, 韩兵强, 魏佳炜, 钟虎堂, 赵浩浩, 段俊龙
Effects of recycled Al
2O
3-C composite slide gate material addition on properties of Al
2O
3-SiC-C castables
Chen Cong, Han Bingqiang, Wei Jiawei, Zhong Hutang, Zhao Haohao, Duan Junlong
耐火材料
.
2025, (6): 471
-476
.