多尺度级配的氧化铝对氧化铝坩埚性能的影响
欧阳李, 杨爽, 顾华志
Effect of multi-scale gradation alumina on performance of alumina crucibles
Ouyang Li, Yang Shuang, Gu Huazhi
耐火材料 . 2025, (6): 495 -499 .  DOI: 10.3969/j.issn.1001-1935.2025.06.007