邻苯二甲酸二辛酯与酚醛树脂对镁尖晶石滑板性能的影响
李强, 曾庆洋, 梁保青, 刘新红, 曾宪新, 王大军
Influence of dioctyl phthalate and phenolic resin on magnesium spinel sliding gate performance
Li Qiang, Zeng Qingyang, Liang Baoqing, Liu Xinhong, Zeng Xianxin, Wang Dajun
耐火材料 . 2025, (6): 521 -524 .  DOI: 10.3969/j.issn.1001-1935.2025.06.012