微孔刚玉骨料对刚玉-尖晶石浇注料性能的影响
谭鑫宇, 王刚, 冯海霞, 柳军, 李传浩, 冯志源
Effect of microporous corundum aggregates on properties of corundum-spinel castables
Tan Xinyu, Wang Gang, Feng Haixia, Liu Jun, Li Chuanhao, Feng Zhiyuan
耐火材料 . 2025, (6): 525 -529 .  DOI: 10.3969/j.issn.1001-1935.2025.06.013