轻量化镁砂制备水泥窑烧成带用方镁石-铁铝尖晶石材料
孙格格, 李国华, 邓舒丹, 田琳
Preparation of lightweight periclase-hercynite refractories with lightweight magnesia for firing zone of cement kilns
Sun Gege, Li Guohua, Deng Shudan, Tian Lin
耐火材料
.
2026, (1): 13
-18
.
DOI: 10.3969/j.issn.1001-1935.2026.01.003