无水硼砂对Al
2O
3-C复合材料性能与显微结构的影响
吴嵩, 韦龙杰, 王建筑, 陈继, 袁愈辉, 刘诚
Effects of anhydrous borax on properties and mircostructure of Al
2O
3-C composites
Wu Song, Wei Longjie, Wang Jianzhu, Chen Ji, Yuan Yuhui, Liu Cheng
耐火材料
.
2026, (1): 65
-68
.
DOI: 10.3969/j.issn.1001-1935.2026.01.012