氧化铝微粉多级配比对刚玉浇注料中低温性能的影响
李冬梅, 李桂梅, 颜林, 李红超, 李璐, 叶青, 邵长波, 陈志强
Effect of multi-fraction gradation of alumina ultrafines on medium and low temperature properties of corundum castables
Li Dongmei, Li Guimei, Yan Lin, Li Hongchao, Li Lu, Ye Qing, Shao Changbo, Chen Zhiqiang
耐火材料
.
2026, (1): 74
-77
.
DOI: 10.3969/j.issn.1001-1935.2026.01.014