碳化硅基复合材料增强增韧研究进展
王鹏睿, 程本军, 梁效诚, 陈方, 吴锋
Research progress on reinforcement and toughening of silicon carbide-based composites
Wang Pengrui, Cheng Benjun, Liang Xiaocheng, Chen Fang, Wu Feng
耐火材料 . 2026, (1): 82 -87 .  DOI: 10.3969/j.issn.1001-1935.2026.01.016