致密方镁石-镁橄榄石复合骨料的制备及性能研究
苑小舟, 曹瑞琦, 马北越, 吕才文, 杨欣
Preparation and properties of dense periclase-forsterite composite aggregates
Yuan Xiaozhou, Cao Ruiqi, Ma Beiyue, Lyu Caiwen, Yang Xin
耐火材料 . 2026, (2): 108 -112 .  DOI: 10.3969/j.issn.1001-1935.2026.02.004