硼砂对高钛无氟型保护渣熔融结晶性能的影响
李涛, 张宇璐, 张玓, 赫志森, 王卫, 刘磊
Effect of borax on melting and crystallization properties of high-titanium fluorine-free mold fluxes
Li Tao, Zhang Yulu, Zhang Di, He Zhisen, Wang Wei, Liu Lei
耐火材料 . 2026, (2): 146 -150 .  DOI: 10.3969/j.issn.1001-1935.2026.02.011