基于流变优化的氧化铝轻质隔热耐火材料3D打印制备
张淳, 吴滨
3D printing preparation of lightweight thermal insulation alumina refractories based on rheological optimization
Zhang Chun, Wu Bin
耐火材料 . 2026, (2): 151 -155 .  DOI: 10.3969/j.issn.1001-1935.2026.02.012