助熔剂对煤矸石基发泡陶瓷性能的影响
张祥飞, 娄广辉, 张梦真, 李静, 张碗玉, 张艺升, 孙茂泽
Effect of fluxes on properties of gangue-based foamed ceramics
Zhang Xiangfei, Lou Guanghui, Zhang Meng-zhen, Li Jing, Zhang Wanyu, Zhang Yisheng, Sun Maoze
耐火材料 . 2026, (2): 156 -160 .  DOI: 10.3969/j.issn.1001-1935.2026.02.013