莫来石/硅酸钇复合涂层制备与性能研究
闵志宇, 袁洪跃, 陈毛, 陈勇强, 范冰冰
Preparation and performance of mullite/yttrium silicate composite coatings
Min Zhiyu, Yuan Hongyue, Chen Mao, Chen Yongqiang, Fan Bingbing
耐火材料
.
2026, (4): 311
-319
.
DOI: 10.3969/j.issn.1001-1935.2026.04.007